MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Lehvoss LUVOCOMĀ® 50/CF/10/TF/15/BK 100 Polycarbonate with carbon fiber and PTFE
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Carbon + PTFE Filled

Material Notes: Properties/attributes include: Very strong and stiff parts; low coefficient of thermal expansion. Electrically conductive, suitable for continuous discharging of statically-generated electricity. Improved friction and wear behavior. Emergency (dry) running property. High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance range.

Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical engineering. Typical uses include: Body and duty parts in office equipment, gear wheels, grippers.

Processing: During processing, the moisture level should not exceed 0.02%, otherwise molecular degradation may occur. Suitable heat treatment may increase resistance to the formation of stress cracks. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application.

Information provided by Lehmann & Voss & Co.KG

Vendors:
Available Properties
  • Specific Gravity, ISO 1183
  • Moisture Absorption
  • Linear Mold Shrinkage, DIN 16901
  • Melt Flow, ISO 1133
  • Tensile Strength, ISO 527-2
  • Elongation at Break, ISO 527-2
  • Modulus of Elasticity, ISO 527-2
  • Flexural Strength, ISO 178
  • Flexural Modulus, ISO 178
  • Flexural Strain at Break, ISO 178, Flexural Elongation @ Fmax
  • Charpy Impact Unnotched, ISO 179
  • Charpy Impact Unnotched, ISO 179 1fu
  • Charpy Impact, Notched, ISO 179 eA
  • Charpy Impact, Notched, ISO 179 1eA
  • Electrical Resistivity, IEC 60167
  • Surface Resistance, IEC 60093
  • CTE, linear, DIN 53752
  • Thermal Conductivity, DIN 52612
  • Maximum Service Temperature, Air, UL 746B, Continuous
  • Maximum Service Temperature, Air, Short Term
  • Vicat Softening Point, DIN ISO 306, VST A
  • Nozzle Temperature
  • Zone 1
  • Zone 2
  • Zone 3
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature, Dehumidifying dryer
  • Moisture Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Lehvoss; Lehmann & Voss & Co.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.