MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
KLJ Group KANATOL FLAMEGUARD C 70 Phosphate Esters
Categories: Fluid

Material Notes: Properties: TCP-70 is the most efficient plasticizer to the liquid tri aryl phosphate type. It is color less to pale yellow liquid insoluble in water & soluble in benzene, toluene etc.

Application: It is low volatile, having good resistance to saponification and oil extraction hence used as a lubricant in adhesives for extreme pressure and fire risk from heat source and electrical sparks. TCP-70 is mainly used as flame retardant plasticizer in many plastics & reins for the application of manufacturing electrical & automobile parts. TCP-70 is used in flame retardant formulations or as an additive in cellulose, polyester and polyurethane. TCP-70 is used in styrenic thermoplastics as an alternative to halogenated flame retardant.

Chemical Name: TRI CRESYL PHOSPHATE (TCP)

Molecular Formula: C 20 H19 O 4 P

CAS Number: 26444-49-5

UN. NO.: 3082

EINECS NO.: 247-693-8

Information provided by KLJ Group

Vendors:
Available Properties
  • Specific Gravity, ASTM D1045-08
  • Brookfield Viscosity, ASTM D445
  • Molecular Weight
  • Refractive Index, ASTM D1045-08
  • Moisture Content, ASTM E203-01
  • Phosphorus, P, KLJ/QCD/WIN/49
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.