MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond MasterSil 323 Two component, addition cured silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Key Features:
  • Convenient handling
  • Optically clear in thin sections
  • Low to moderate viscosity
  • Excellent strength properties
Product Description: Master Bond MasterSil 323 is a two component silicone for high performance bonding, sealing, and encapsulating. It does not require air when polymerizing and does not outgas while curing. It has a forgiving one to one mix ratio by weight. The viscosity of both Parts A and B allows for easy mixing and good flow. It is a low exothermic material with a long open time of about 2-3 hours. It cures at ambient temperatures in 48-72 hours or in 2-4 hours at 135- 165°F. The optimum cure is overnight at room temperature followed by 2-4 hours at 135-165°F. This silicone contains no solvents or diluents and has very low shrinkage upon curing. It has a Shore A hardness of 35 to 45. MasterSil 323 bonds well to a wide variety of substrates including metal, glass, plastics and ceramics, as well as to silicone rubber. It can withstand the most rigorous kinds of thermal shock and cycling without cracking or exerting stress on components. The service temperature range is from -65°F to +400°F. Other noteworthy features are its optical clarity, especially in thinner sections, and its superior electrical insulation profile. MasterSil 323 should be considered in optical, electronic, aerospace, and specialty OEM applications where a high strength, optically clear, easy to use, silicone is needed.

Product Advantages:

  • Addition cured, no by-products released during cure
  • Flowable, with long open time
  • Optically clear, especially in thin sections
  • Good bond strength, yet potentially removable
  • Low dielectric constant

Information provided by Master Bond.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, Part A
  • Hardness, Shore A
  • Tensile Strength
  • Elongation at Break
  • Tensile Modulus
  • Adhesive Bond Strength, Tensile lap shear, Al to Al
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Refractive Index
  • Cure Time, Optimum: Overnight at 75°F followed by 2-4 hours at 135-165°F
  • Cure Time, Option 2
  • Cure Time, Option 1
  • Working Life, after mixing, 100 gram batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.