Veradel® 3300 SL30 is a polyethersulfone (PESU) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and externally lubricated applications. The resin is formulated with a ternary anti-friction/anti-wear additive system comprised of carbon fiber, graphite, and polytetrafluoroethylene (PTFE). Veradel® PESU is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent wear resistance, ease of melt processing, high purity, and excellent chemical resistance. These properties make it well-suited for applications in transportation, electronics, chemical processing, and industrial uses. The resin is black in color in its natural state. Applications: Automotive Applications; Bearings; Bushings; Gears; Industrial Applications; Profiles; Rods; Sheet Features: Chemical Resistant; Good Dimensional Stability; High Heat Resistance; Low Friction; Medium Flow; Wear Resistant Information provided by Solvay Specialty Polymers. |