MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Sika SikaBond® T35 Trowel-applied, Polyurethane Wood Flooring Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: SikaBond-T35 is a one-component, low-VOC, low odor, moisture cured polyurethane adhesive for full surface bonding of wood flooring. SikaBond-T35 will tenaciously bond wood to most surfaces, including concrete, plywood, and leveling and patch underlayments that have been properly prepared.

Where to Use: SikaBond-T35 may be used to bond all engineered, solid plank flat milled, shorts up to max. 3/4” thick, including bamboo, cork and parquet hardwood flooring designed by the manufacturer for glue down applications. This adhesive can also be used for many other bonding applications that are common for light commercial and residential applications including acoustic rubber underlayment systems.

Advantages:

  • 170% Elongation
  • Low odor
  • Easy to trowel
  • Excellent workability
  • Fast curing
  • Crack bridging
  • Suitable for common types of wood floors
  • Suitable for in-floor radiant heat installation
  • Contains no water
  • Tenacious bond

Information provided by Sika Corporation.

Vendors:
Available Properties
  • Density
  • Volatile Organic Compounds (VOC) Content
  • Hardness, Shore A, after 28 days
  • Tensile Strength
  • Elongation at Break, 50% RH
  • Shear Strength, 1 mm adhesive thickness at 73°F (23°C) and 50% RH
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, 50% RH, Skinning/Laying time
  • Cure Time, Floor may accept light foot traffic depending on climatic conditions and adhesive layer thickness
  • Cure Time, 50% RH
  • Shelf Life, in original unopened cartridge
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.