Applications:- Blood Therapy
- Dialyzer Housings
- IV Components
Key Attributes: - Ease of processing
- Excellent clarity
- Excellent hydrolytic stability
- Fast drying times
- Good chemical resistance
- Outstanding impact resistance
- Quick cycle times
Product Description:Eastman Tritan MX810 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistance. This new generation copolyester can also be molded into various applications without incorporating high levels of residual stress. Eastman Tritan Copolyester MX810 has been tested for FDA/ISO 10993 and USP Class VI Biological Evaluation testing after Gamma and ETO sterilization. Information provided by Eastman. |