MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chromium Copper, UNS C18500, TH08 Temper 4 mm rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability; good hot workability.

Applications: resistance welding electrodes, seam welding wheels, switch gear, electrode holder jaws, cable connectors, current carrying arms and shafts, circuit breaker parts, molds, spot welding tips, flash welding electrodes, electrical and thermal conductors requiring strength, switch contacts.

Test specimen: rod - 4mm diameter.

UNS C18500 is inactive per the Copper Development Association. UNS C18200, UNS C18400, and UNS C18500 have similar compositions and mechanical properties.

Key Words: CDA 185, CA185
Vendors:
Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break, In 50 mm
  • Modulus of Elasticity
  • Poissons Ratio
  • Machinability, UNS C36000 (free-cutting brass) = 100%
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity, TB00 temper
  • Melting Point
  • Solidus
  • Liquidus
  • Solution Temperature, For 10-30 minutes, water quench
  • Aging Temperature, For 2-4 hours
  • Hot-Working Temperature
  • Chromium, Cr
  • Copper, Cu
  • Lead, Pb
  • Lithium, Li
  • Phosphorus, P
  • Silver, Ag
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.