MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Proto3000 Copper C18150 Processed by DMSL
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Copper Alloy

Material Notes: Highlights:
  • Chromium Zirconium Copper (CuCr1Zr)
  • Excellent electrical and thermal conductivity
  • mechanical and material properties stable up to 700°F
  • Age Hardenable
Applications:
  • Excellent thermal and electrical conductivity
  • Conformal induction coils
  • Regeneratively cooled nozzles
  • Plastic mold components

Information provided by Proto3000

Key Words: Direct Metal Laser Sintering
Vendors:
Available Properties
  • Hardness, Rockwell B, Z Axis, SR + Hot Isostatic Press (HIP)
  • Hardness, Rockwell B, Z Axis, SR + HIP + SHT + Precipitation Strengthening (PHT)
  • Hardness, Rockwell B, Z Axis, As Built
  • Hardness, Rockwell B, Z Axis, SR + HIP + Solution Anneal (SHT)
  • Hardness, Rockwell B, Z Axis, Stress Relief (SR)
  • Tensile Strength, Ultimate, Z Axis, As Built
  • Tensile Strength, Ultimate, Z Axis, Stress Relief (SR)
  • Tensile Strength, Ultimate, Z Axis, SR + Hot Isostatic Press (HIP)
  • Tensile Strength, Ultimate, Z Axis, SR + HIP + Solution Anneal (SHT)
  • Tensile Strength, Ultimate, Z Axis, SR + HIP + SHT + Precipitation Strengthening (PHT)
  • Tensile Strength, Yield, Z Axis, SR + Hot Isostatic Press (HIP)
  • Tensile Strength, Yield, Z Axis, SR + HIP + Solution Anneal (SHT)
  • Tensile Strength, Yield, Z Axis, As Built
  • Tensile Strength, Yield, Z Axis, Stress Relief (SR)
  • Tensile Strength, Yield, Z Axis, SR + HIP + SHT + Precipitation Strengthening (PHT)
  • Elongation at Break, Z Axis, Stress Relief (SR)
  • Elongation at Break, Z Axis, As Built
  • Elongation at Break, Z Axis, SR + HIP + SHT + Precipitation Strengthening (PHT)
  • Elongation at Break, Z Axis, SR + Hot Isostatic Press (HIP)
  • Elongation at Break, Z Axis, SR + HIP + Solution Anneal (SHT)
  • Tensile Modulus, Z Axis, Stress Relief (SR)
  • Tensile Modulus, Z Axis, As Built
  • Tensile Modulus, Z Axis, SR + HIP + Solution Anneal (SHT)
  • Tensile Modulus, Z Axis, SR + Hot Isostatic Press (HIP)
  • Tensile Modulus, Z Axis, SR + HIP + SHT + Precipitation Strengthening (PHT)
  • Chromium, Cr
  • Nitrogen, N
  • Other, total
  • Oxygen, O
  • Zirconium, Zr
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.