Chitin nanogel has rich functional groups, can be redispersed after drying, and has good biological safety and compatibility. It has broad application prospects in agriculture, medicine, food, beauty and health care, sensors and other fields. NAT-1510; Chitin Nanogel Morphology: Powder |