MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Geon® Performance Solutions Vinyl Packaging RB-FG Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Geon® RB-FG is a clear, rigid PVC compound designed specifically for use as a color/ stability booster additive in Geon® packaging compounds where high regrind usage is necessary in extrusion blow molding application. Geon® RB-FG is formulated for use in general purpose and food grade appliactions when used according to conditions under Recommended Use

Recommended Use - The actual use level depends on the condition of the regrind, level of regrind, and the desired appearance of the blow molded bottle. A suggested starting range would be 2% to 4% of the virgin and regrind blend. Anything over 4% use level should be discussed with a PolyOne Packaging Compound technical representative to be sure the containers or parts remain compliant to FDA regulations

Geon Performance Solutions was created from PolyOne in 2019.

Vendors:
Available Properties
  • Volatiles
  • Apparent Bulk Density, ASTM D1505
  • FDA, Food Contact, Unspecified Rating
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.