MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Total PPR 6575 Polypropylene, Random Copolymer, Film Grade
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Color. Low catalyst residuals in TOTAL Petrochemicals 6575 polypropylene results in improved color stability.

Clarity/Impact. The random copolymer structure of 6575 improves its clarity and resiliency over conventional homopolymer films.

FDA. 6575 complies with all applicable FDA regulations for food contact applications.

Recommended Applications. 6575 is recommended for use in manufacture of packaging films that require improved optical and resiliency or special surface attributes.

Information provided by Total Petrochemicals.

Vendors:
Available Properties
  • Specific Gravity, ASTM D1505
  • Water Vapor Transmission, ASTM F1249-90, 90% RH
  • Melt Flow, ASTM D1238
  • Tensile Strength at Break, ASTM D882, non-oriented film
  • Elongation at Break, ASTM D882
  • Dart Drop, ASTM D1709
  • Melting Point, DSC
  • Haze, ASTM D1003
  • Gloss, ASTM D2457, at 45°
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Total Atofina

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.