MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Freudenberg N431 Nitrile Elastomer (NBR)  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: General Purpose; Internal Lubricant. Inferior resistance to ozone, sunlight and natural aging; poor resistance to oxygenated solvents. All testing done on AS568-214 size o-rings

This product was formerly sold under the Freudenberg Simrit division; now Freudenberg Sealing Technologies.

Key Words: CHEMIGUM® , HYCAR® , PARACRIL® , PERBUNAN®, KRYNAC®, NYSYSN®
Vendors:
Available Properties
  • Hardness, Shore A, ASTM D2240, Original Properties
  • Hardness, Shore A, ASTM D2240, ASTM Reference Fuel B Immersion, 70 hours
  • Hardness, Shore A, ASTM D2240, ASTM Fuel A Immersion, 70 hours
  • Hardness, Shore A, ASTM D2240, Air Aging, 70 hours
  • Hardness, Shore A, ASTM D2240, ASTM IRM-903 Oil Immersion, 70 hours
  • Hardness, Shore A, ASTM D2240, Water Resistance, 70 hours
  • Tensile Strength, Ultimate, ASTM D412 Die C, Original Properties
  • Tensile Strength, Ultimate, ASTM D412 Die C, ASTM Reference Fuel B Immersion, 70 hours
  • Tensile Strength, Ultimate, ASTM D412 Die C, ASTM Fuel A Immersion, 70 hours
  • Tensile Strength, Ultimate, ASTM D412 Die C, Air Aging, 70 hours
  • Tensile Strength, Ultimate, ASTM D412 Die C, ASTM IRM-903 Oil Immersion, 70 hours
  • Elongation at Break, ASTM D412 Die C, Original Properties
  • Elongation at Break, ASTM D412 Die C, ASTM Reference Fuel B Immersion, 70 hours
  • Elongation at Break, ASTM D412 Die C, Air Aging, 70 hours
  • Elongation at Break, ASTM D412 Die C, ASTM IRM-903 Oil Immersion, 70 hours
  • Elongation at Break, ASTM D412 Die C, ASTM Fuel A Immersion, 70 hours
  • Compression Set, ASTM D395
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.