| LI2516 is a pelleted linear low density polyethylene with very narrow molecular weight distribution. Applications: House-wares, lids, closures and toys. Advantages: Excellent stress crack resistance, toughness and gloss, superior molding properties, low odor. Information provided by Titan Chemicals |