MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Soarus SoarnoL® ST110 Ethylene Vinyl Alcohol Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Alcohol (EVOH)

Material Notes: Modified DC3203; improved flex crack resistance and thermoformability. Ethylene content 32 mol%. Volatile matter 0.3%.

The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a thin gas barrier layer without loss of shelf life.

Soarnol ST110 has an excellent flex crack resistance and stretchability without lower of gas barrier property. This grade is appropriate for bag-in-box and stretched film.

Information provided by Soarus, LLC, a Mitsubishi Company.

Key Words: EVOH
Vendors:
Available Properties
  • Density
  • Moisture Vapor Transmission, 40°C- 90% RH; based on 30 µm layer
  • Oxygen Transmission, 20°C- 65% RH; based on 20 µm layer
  • Viscosity
  • Melt Flow
  • Melting Point, DSC, both heating and cooling speeds of 20°C/min
  • Crystallization Temperature, DSC, both heating and cooling speeds of 20°C/min
  • Glass Transition Temp, Tg, DSC, both heating and cooling speeds of 20°C/min
  • Refractive Index, Quenched
  • Refractive Index, Annealed at 140°C, 30 min
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Soarus, Mitsubishi

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.