MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Tra-Con Tra-Bond 2115 Clear High Strength Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 2115 is a clear, low viscosity epoxy formulation used in the fabrication of lasers. It is capable of withstanding 30 seconds of 60 watt direct laser energy. The low cure shrinkage (using a room temperature cure) make 2115 an excellent choice for bonding optical components where alignment accuracy is essential. This high strength system is also used for laminating glass and rigid plastics or bonding metals and ceramics. TRA-BOND 2115 offers superior resistance to mechanical shock and temperature cycling. It has been used in cycling applications down to 4K. It is also resistant to water, weather, ozone, most petroleum products, mild acids and alkalis and many other chemicals.

Information provided by Tra-Con Inc.

Vendors:
Available Properties
  • Specific Gravity, Mixed
  • Viscosity, After mixing
  • Hardness, Shore D
  • Adhesive Bond Strength, Lap shear, alum to alum
  • Izod Impact, Notched
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, Ultimate Tg
  • Refractive Index
  • Transmission, Visible, clear; thickness not quantified
  • Cure Time
  • Cure Time
  • Pot Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Tra-Con, Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.