Available Properties |
---|
- Density, Average value: 1.49 g/cc Grade Count:645
- Density, Average value: 1.30 g/cc Grade Count:2
- Filler Content, Average value: 32.7 % Grade Count:167
- Water Absorption, Average value: 0.369 % Grade Count:224
- Moisture Absorption at Equilibrium, Average value: 0.911 % Grade Count:164
- Moisture Absorption at Equilibrium, Average value: 1.08 % Grade Count:24
- Water Absorption at Saturation, Average value: 3.71 % Grade Count:32
- Additive Loading, Average value: 32.2 % Grade Count:30
- Viscosity, Average value: 19.0 cP Grade Count:3
- Viscosity, Average value: 19.0 cP Grade Count:3
- Viscosity Number, Average value: 111 cm³/g Grade Count:5
- Maximum Moisture Content, Average value: 0.0767 Grade Count:3
- Linear Mold Shrinkage, Average value: 0.00418 cm/cm Grade Count:526
- Linear Mold Shrinkage, Transverse, Average value: 0.00799 cm/cm Grade Count:301
- Melt Flow, Average value: 23.0 g/10 min Grade Count:12
- Spiral Flow, Average value: 43.0 cm Grade Count:3
- Hardness, Rockwell M, Average value: 105 Grade Count:3
- Hardness, Rockwell R, Average value: 124 Grade Count:83
- Ball Indentation Hardness, Average value: 307 MPa Grade Count:11
- Tensile Strength, Ultimate, Average value: 184 MPa Grade Count:611
- Tensile Strength, Ultimate, Average value: 133 MPa Grade Count:71
- Tensile Strength, Yield, Average value: 156 MPa Grade Count:93
- Tensile Strength, Yield, Average value: 71.3 MPa Grade Count:11
- Elongation at Break, Average value: 3.56 % Grade Count:656
- Elongation at Break, Average value: 4.94 % Grade Count:68
- Elongation at Yield, Average value: 5.26 % Grade Count:38
- Elongation at Yield, Average value: 6.92 % Grade Count:4
- Modulus of Elasticity, Average value: 13.8 GPa Grade Count:622
- Modulus of Elasticity, Average value: 9.67 GPa Grade Count:79
- Flexural Yield Strength, Average value: 263 MPa Grade Count:539
- Flexural Yield Strength, Average value: 126 MPa Grade Count:24
- Flexural Yield Strength, Average value: 126 MPa Grade Count:4
- Flexural Yield Strength, Average value: 126 MPa Grade Count:4
- Flexural Modulus, Average value: 12.3 GPa Grade Count:554
- Flexural Modulus, Average value: 6.35 GPa Grade Count:48
- Flexural Strain at Break, Average value: 2.61 % Grade Count:28
- Flexural Strain at Break, Average value: 4.48 % Grade Count:1
- Compressive Yield Strength, Average value: 197 MPa Grade Count:36
- Compressive Yield Strength, Average value: 171 MPa Grade Count:2
- Poissons Ratio, Average value: 0.357 Grade Count:48
- Fatigue Strength, Average value: 100 MPa Grade Count:4
- Fatigue Strength, Average value: 100 MPa Grade Count:4
- Shear Modulus, Average value: 3.15 GPa Grade Count:12
- Shear Modulus, Average value: 1.75 GPa Grade Count:3
- Shear Strength, Average value: 79.4 MPa Grade Count:56
- Secant Modulus, Average value: 10.1 GPa Grade Count:1
- Secant Modulus, Average value: 10.1 GPa Grade Count:1
- Izod Impact, Average value: 76.3 J Grade Count:28
- Izod Impact, Notched, Average value: 1.04 J/cm Grade Count:326
- Izod Impact, Notched, Average value: 2.23 J/cm Grade Count:3
- Izod Impact, Unnotched, Average value: 6.22 J/cm Grade Count:249
- Izod Impact, Notched (ISO), Average value: 13.2 kJ/m² Grade Count:156
- Izod Impact, Notched (ISO), Average value: 15.1 kJ/m² Grade Count:22
- Izod Impact, Unnotched (ISO), Average value: 53.7 kJ/m² Grade Count:111
- Izod Impact, Unnotched (ISO), Average value: 54.1 kJ/m² Grade Count:11
- Charpy Impact Unnotched, Average value: 6.47 J/cm² Grade Count:254
- Charpy Impact Unnotched, Average value: 5.59 J/cm² Grade Count:74
- Charpy Impact, Notched, Average value: 1.21 J/cm² Grade Count:257
- Charpy Impact, Notched, Average value: 1.19 J/cm² Grade Count:71
- Gardner Impact, Average value: 10.2 J Grade Count:3
- Dart Drop, Total Energy, Average value: 12.0 J Grade Count:24
- Falling Dart Impact, Average value: 7.52 J Grade Count:8
- Instrumented Impact Total Energy, Average value: 2.62 J Grade Count:6
- Coefficient of Friction, Average value: 0.332 Grade Count:24
- Coefficient of Friction, Static, Average value: 0.310 Grade Count:24
- Tensile Creep Modulus, 1 hour, Average value: 9420 MPa Grade Count:6
- Tensile Creep Modulus, 1000 hours, Average value: 8000 MPa Grade Count:6
- K (wear) Factor, Average value: 1150 x 10-8 mm³/N-M Grade Count:27
- Dynatup @ -18°C, Average value: 53.3 J Grade Count:3
- Dynatup @ -18°C Max Load, Average value: 524000 g Grade Count:3
- Electrical Resistivity, Average value: 2.94e+15 ohm-cm Grade Count:270
- Surface Resistance, Average value: 2.60e+15 ohm Grade Count:107
- Static Decay, Average value: 2.00 sec Grade Count:4
- Dielectric Constant, Average value: 4.22 Grade Count:105
- Dielectric Constant, Average value: 30.5 Grade Count:2
- Dielectric Constant, Average value: 30.5 Grade Count:2
- Dielectric Strength, Average value: 27.3 kV/mm Grade Count:119
- Dielectric Strength, Average value: 9.56 kV/mm Grade Count:2
- Dissipation Factor, Average value: 0.0137 Grade Count:89
- Dissipation Factor, Average value: 0.277 Grade Count:2
- Dissipation Factor, Average value: 0.277 Grade Count:2
- Arc Resistance, Average value: 160 sec Grade Count:21
- High Voltage Arc Resistance to Ignition (HVAR), Average value: 95.0 sec Grade Count:3
- Comparative Tracking Index, Average value: 572 V Grade Count:157
- Hot Wire Ignition, HWI, Average value: 127 sec Grade Count:9
- High Amp Arc Ignition, HAI, Average value: 101 arcs Grade Count:9
- High Voltage Arc-Tracking Rate, HVTR, Average value: 15.0 mm/min Grade Count:19
- CTE, linear, Average value: 27.8 µm/m-°C Grade Count:175
- CTE, linear, Average value: 27.9 µm/m-°C Grade Count:62
- CTE, linear, Transverse to Flow, Average value: 59.5 µm/m-°C Grade Count:110
- CTE, linear, Transverse to Flow, Average value: 93.8 µm/m-°C Grade Count:63
- Specific Heat Capacity, Average value: 1.51 J/g-°C Grade Count:4
- Specific Heat Capacity, Average value: 2.65 J/g-°C Grade Count:2
- Thermal Conductivity, Average value: 2.30 W/m-K Grade Count:23
- Thermal Conductivity, Average value: 0.245 W/m-K Grade Count:2
- Melting Point, Average value: 311 °C Grade Count:257
- Maximum Service Temperature, Air, Average value: 180 °C Grade Count:65
- Deflection Temperature at 0.46 MPa (66 psi), Average value: 273 °C Grade Count:150
- Deflection Temperature at 1.8 MPa (264 psi), Average value: 258 °C Grade Count:529
- Deflection Temperature at 8.0 MPa, Average value: 187 °C Grade Count:31
- Vicat Softening Point, Average value: 249 °C Grade Count:46
- Glass Transition Temp, Tg, Average value: 98.3 °C Grade Count:43
- UL RTI, Electrical, Average value: 132 °C Grade Count:19
- UL RTI, Mechanical with Impact, Average value: 107 °C Grade Count:10
- UL RTI, Mechanical without Impact, Average value: 123 °C Grade Count:10
- Flammability, UL94, Grade Count:344
- Flammability, UL94, Grade Count:1
- Flame Spread, Average value: 64.3 mm/min Grade Count:16
- Oxygen Index, Average value: 29.1 % Grade Count:20
- Glow Wire Test, Average value: 828 °C Grade Count:28
- Transmission, Visible, Average value: 29.5 % Grade Count:4
- Reflection Coefficient, Visible (0-1), Average value: 0.900 Grade Count:5
- Processing Temperature, Average value: 316 °C Grade Count:71
- Nozzle Temperature, Average value: 327 °C Grade Count:36
- Melt Temperature, Average value: 320 °C Grade Count:456
- Mold Temperature, Average value: 133 °C Grade Count:487
- Drying Temperature, Average value: 110 °C Grade Count:413
- Moisture Content, Average value: 0.0717 % Grade Count:320
- Dew Point, Average value: -30.9 °C Grade Count:119
- Injection Pressure, Average value: 93.7 MPa Grade Count:177
|
| | |