MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Lanxess LEWATIT® TP 208 Cation Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® TP 208 is a weakly acidic, macroporous cation exchange resin with chelating imino-diacetat groups for the selective removal of alkaline earth cations. Lewatit TP 208 has a heterodispersed bead size. In comparison to Lewatit TP 207 and Lewatit MonoPlus TP 207 this resin has a modified polymer structure and also a modified substitution grade of the imino-diacetate groups to make it especially suitable for the adsorption of earth alkali ions in the presence of alkali ions. It is especially suitable for use in: final polishing of brine feed to chloraklai membrane cells (traces of alkaline earth ions are removed after their normal precipitation by carbonates in the pH-range 8-11) in the presence of iron (III) ions and in case Sr and Ba have also to be removed besides Ca and Mg. The operating capacity of Lewatit TP 208 depends on the pH-value of the brine. At pH 10 it is approx. three fold of that achieved at pH 7. At pH 10 and calcium content of 5 ppm, an operating capacity of approx. 12 g Ca/l Lewatit TP 208 (volume of resin in di-sodium-form) is obtained. At a service flow rate of 20-30 BV/h, the residual calcium concentration is well below 20 ppb. Greater security can be achieved by operating two units of equal size in series. Lewatit TP 208 has to be conditioned with caustic soda solution after every regeneration cycle/before every exhaustion cycle. After the conditioning it is in di-sodium-form and ready to use for the final polishing of chlorakali brine feed. Aside from its major application in brine purification Lewatit TP 208 can be used for the removal or recovery of heavy metals out of process-, waste water- and potable water streams. Thereby, it removes heavy metal cations from neutralized aqueous solutions in the following order: Copper>Vanadium (VO2)>Uranium (UO2)>Lead>Nickel>Zinc>Cadmium>Iron (II)>Beryllium>Manganese> Calcium>Magnesium>Strontium>Barium>Sodium. Lewatit TP 208 does not remove heavy metals from solutions containing EDTA or NTA respectively. Only cadmium is removed from solutions containing cyanides.

Information provided by Lanxess.

Vendors:
Available Properties
  • Bulk Density
  • Density
  • Bead Size, Mean
  • Storage Temperature
  • Maximum Service Temperature, Air
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Lanxess, Spinoff of Bayer

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.