MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Latrobe Dynamax™ ASTM M42, DIN 1.3247 Super High Speed Steel
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Tool Steel

Material Notes: Dynamax super high speed steel is a premium cobalt high speed steel with a chemical composition designed for high hardness and superior hot hardness. These properties make the steel an excellent choice for machining high-strength and prehardened steels, high-hardness alloys, and the difficult-to-machine, nonferrous superalloys used in the aerospace, oil, and power generation industries. Dynamax super high speed steel exhibits excellent wear resistance by virtue of high heat-treated hardness (68 to 70 HRC), and the high cobalt content imparts the hot hardness. As such, the cutting edges on tools made from Dynamax super high speed steel stay sharp and hard in heavy-duty and high-production cutting applications. Typical applications for Dynamax super high speed steel include twist drills, taps, milling cutters, reamers, broaches, saws, knives, and thread rolling dies.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Hardness, Rockwell C, Oil Quenched from 1204°C, 5 minutes
  • Hardness, Rockwell C, Oil Quenched from 1177°C, 5 minutes
  • Hardness, Rockwell C, Oil Quenched from 1163°C
  • Modulus of Elasticity
  • Machinability, 1% Carbon Steel
  • Izod Impact Unnotched, Oil Quenched at 1191°C; 510°C Temper Temperature
  • Izod Impact Unnotched, Oil Quenched at 1191°C; 622°C Temper Temperature
  • Processing Temperature, Critical Temperaure Ac1
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co
  • Iron, Fe
  • Molybdenum, Mo
  • Silicon, Si
  • Tungsten, W
  • Vanadium, V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Latrobe Steel

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.