Product Description: Nucrel™ 0403 is a copolymer of ethylene and methacrylic acid, made with nominally 4% methacrylic acid. The resin is available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Uses: Adhesives; Packaging; Sealants Composition: 4% by weight Methacrylic Acid comonomer content Availability: Africa 7 Middle East; Asia Pacific; Europe; Latin America; North America Agency Ratings: FDA 21 CFR 177.1330 (a) Form: Pellets Processing Method: Blown Film; Cast Film; Coextrusion; Extrusion Information provided by The Dow Chemical Company |