MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Northstar Polymers MSB-M25F Microcellular Foam based on High Performance Polyester Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: This high performance polyester microcellular foam system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane foams molded with this system exhibit high tear strength, excellent oil resistance, and outstanding abrasion resistance. They also meet the requirements of 21 CFR 177.1680, FDA direct dry food contact. When the packing factor exceeds 1, an integral skin will develop with properties approaching those of the cast elastomer. For long-term use in constant aqueous environments, consider a polyether or hybrid product system.

Information provided by Northstar Polymers.

Vendors:
Available Properties
  • Density, Free Rise Density
  • Density, Packing Density
  • Hardness, Shore A, ASTM D2240
  • Rebound, ASTM D2632, Bashore Rebound
  • Processing Temperature, Prepolymer Temperature
  • Processing Temperature, Curing Agent Temperature
  • Mold Temperature
  • Cure Time, De-mold Time
  • Cure Time, Complete Cure Cycle
  • Cure Time, Complete Cure Cycle
  • Pot Life
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.