MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
SEKISUI SPI KYDEX® 110 Polymer Alloy Sheet
Categories: Polymer; Thermoplastic

Material Notes: Metallic fire-rated sheet

Super tough, durable KYDEX® 110, a proprietary alloy sheet, brings new dimensions to thermoformers in: formability, rigidity, breakage resistance, chemical resistance and fire retardancy.

This high performance thermoplastic sheet is available in an assorted number of metallic colors. It is Underwriters Laboratories, Inc® recognized for UL Std 94 V-0, 5V.

Suggested Applications:

  • Aircraft Interiors
  • Kiosk Housings
  • Medical Housings
  • Miscellaneous Applications
  • Exhibits and Displays
  • Store Fixtures
  • Office Furniture

Features:

  • For deep or hard to form parts where good finished detail is required
  • More rigid than most thermoplastics so parts will deform less when loaded
  • Meets highest standard for chemical resistance for thermoplastic materials
  • Recognized by Underwriter's Laboratories, Inc® for Std 94 V-0, 5V in all thicknesses and colors
  • Excellent forming properties, uniform wall thicknesses
  • Easy machining and fabricating using conventional methods and equipment
  • Passes FFA Vertical Burn Testing according to FAR 25.853 (a) (i)+(ii)

Values based upon 3.18 mm (0.125 in) sheet unless otherwise specified.

Information provided by Sekisui Polymer Innovations

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Tensile Strength, ASTM D638
  • Modulus of Elasticity, ASTM D790
  • Flexural Strength, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Annealed
  • Flammability, UL94, UL File E115252; Component Recognition
  • Flammability, UL94, UL Standard 94, Underwriters Laboratories., Inc®, File E115252; Component Recognition
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.