Product Description: 85 Shore A TPE (Styrenic Block Copolymer based) available in black and natural for extrusion applications. This grade offers good melt strength, low coefficient of friction, UV performance and good sealing characteristics. Availability: North America Features: Acid Resistant; Alcohol Resistant; Base Resistant; Detergent Resistant; Good Adhesion; Good Colorability; Good Melt Strength; Good Processability; High Elasticity; Low Compression Set; Low Friction; Oil Resistant; Ozone Resistant; Recyclable Material; Solvent Resistant; UV Resistant Appearance: Black; Natural Color Processing Method: Extrusion; Injection Molding Information provided by Entec Polymers |