MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Honeywell HT5000 Thermally Conductive Gap Fillers
Categories: Polymer; Thermoset; Silicone

Material Notes: Benefits And Features:
  • High thermal performance
  • low contact resistance
  • Easily dispensable and reworkable
  • High compressibility for low stress applications
  • Reliable thermal performance
  • No pump out and cracking risk
Overview: Honeywell HT one-part series Gap Filler provides an effective thermal properties and high conformability with its high compressibility. It is formulated to deliver high dispense rates for improved productivity, long-term reliability performance and easy reworkability. It is designed to minimize thermal resistance at interfaces, maintain excellent performance through reliability testing, and provide scalable application at a competitive cost.

Typical Applications:

  • Consumer electronics
  • Telecommunications equipment
  • Automotive electronics
  • Power supplies & semiconductors
  • Memory & power modules
  • Power electronics

Information provided by Honeywell

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Outgassing - Total Mass Loss, ASTM E595
  • Thermal Conductivity, ASTM D5470
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.