MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Chesterton 622 White Grease
Categories: Fluid; Lubricant; Aluminum Gellant

Material Notes: Chesterton® 622 White Grease is a pure mineral oil grease with PTFE added designed for applications where a clean, nonstaining, food grade lubricant is required. It is a superior, multipurpose product that conforms with FDA regulation 178.3570 and 177.1550 for food machinery use. It is NSF registered as an H1 lubricant and can be used in federally inspected meat and poultry plants. It is a long lasting, non-hardening lubricant that withstand washout from water, steam, food or fruit juices. Chesterton 622 White Grease is virtually tasteless and odorless. When used on food processing equipment, users can be assured that the lubricant will not contaminate finished products.

Features:

  • NLGI #2
  • Excellent Water Resistance
  • PTFE Fortified
  • NSF H1 - Registration number 133929

Applications: A superior quality, clean, multi-purpose grease to lubricate slides, guides, moving parts of equipment in food, beverage, pharmaceutical, textile and other plants processing clean materials or packages. Use on bottle filling machinery, carton filling equipment, valves, pistons, pumps, paste and sauce fillers, conveyor belts and rollers, fruit feeders, meat packing equipment, canning machinery etc.

Information provided by Chesterton

Vendors:
Available Properties
  • Specific Gravity
  • Viscosity Measurement, ASTM D445, Base Oil
  • Kinematic Viscosity at 40°C (104°F), ASTM D445, Base Oil
  • Kinematic Viscosity at 100°C (212°F), ASTM D445, Base Oil
  • Four Ball Extreme Pressure, Load Wear Index, ASTM D2596
  • Four Ball Extreme Pressure, Weld Load, ASTM D2596
  • Four Ball Wear, ASTM D2266, Weld Scar Diameter
  • Penetration, ASTM D217
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Dropping Point, ASTM D2265
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.