MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Momentive Performance Materials GE Silicones UltraGlaze SSG4400A + SSG471XB Structural Silicone Glazing Adhesive
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: GE SSG4400 UltraGlaze is a high-modulus neutral curing structural silicone elastomeric adhesive for use in shop, factory and field glazing of curtain wall panels. SSG4400 is a two-component product (part A + part B) that upon mixing, yields rapid and thorough deep-section cure, fast durometer and strength build and quick curing to high strength durable silicone rubber. Performance: Silicone durability, Primerless adhesion, Low pumping viscosity, Fast durometer & strength build. Application: SSG4400 is suitable for use in structural glazing applications such as factory or field glazing of curtain wall units and modules for unitized and panelized systems. SSG4400 is suitable for use as a weather seal product, when movement expected in the joint does not exceed its movement capability (±25%).

Information provided by Momentive Performance Materials.

Vendors:
Available Properties
  • Specific Gravity, SSG4710B
  • Specific Gravity, SSG4713B
  • Specific Gravity
  • Volatile Organic Compounds (VOC) Content, SSG4713B (SSG4710B)
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength, ASTM C1135
  • Elongation, Ultimate, ASTM C1135
  • Shear Strength, ASTM C961
  • Tear Strength, ASTM D624, Die B.
  • Maximum Service Temperature, Air, Heat Resistance
  • Shelf Life, SSG4710B. When stored properly.
  • Shelf Life, SSG4713B. When stored properly
  • Shelf Life, SSG4400A. When properly stored.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Momentive Performance Materials (GE Silicones)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.