MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
SABIC SABIC® HDPE FJ00952 PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: FJ00952 is TNPP additive free grade, high molecular weight High Density Polyethylene copolymer which has a broad molecular weight distribution. The design of the product, molecular architecture and density, gives it a unique combination of easy extrusion and high melt strength with strong physical properties which makes it suitable for producing thin films with excellent strength and rigidity.

Information provided by SABIC

Vendors:
Available Properties
  • Density, ASTM D1505
  • Melt Flow, ASTM D1238
  • Melt Flow, ASTM D1238
  • Film Tensile Strength at Yield, MD, ASTM D882, Properties are based on 15 µm film produced at 4 BUR using 100% FJ00952.
  • Film Tensile Strength at Yield, TD, ASTM D882, Properties are based on 15 µm film produced at 4 BUR using 100% FJ00952.
  • Film Elongation at Break, MD, ASTM D882, Properties are based on 15 µm film produced at 4 BUR using 100% FJ00952.
  • Film Elongation at Break, TD, ASTM D882, Properties are based on 15 µm film produced at 4 BUR using 100% FJ00952.
  • Elmendorf Tear Strength MD, ASTM D1525, Properties are based on 15 µm film produced at 4 BUR using 100% FJ00952.
  • Elmendorf Tear Strength TD, ASTM D1525, Properties are based on 15 µm film produced at 4 BUR using 100% FJ00952.
  • Dart Drop, ASTM D1709, Properties are based on 15 µm film produced at 4 BUR using 100% FJ00952.
  • Film Tensile Strength at Break, MD, ASTM D882, Properties are based on 15 µm film produced at 4 BUR using 100% FJ00952.
  • Film Tensile Strength at Break, TD, ASTM D882, Properties are based on 15 µm film produced at 4 BUR using 100% FJ00952.
  • 1% Secant Modulus, MD, ASTM D882, Properties are based on 15 µm film produced at 4 BUR using 100% FJ00952.
  • 1% Secant Modulus, TD, ASTM D882, Properties are based on 15 µm film produced at 4 BUR using 100% FJ00952.
  • Vicat Softening Point, ASTM D1525
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.