MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Morgan Advanced Ceramics Min-K® K-Shield™ Felt AG Composite Thermal Ceramic
Categories: Ceramic

Material Notes: Min-K - K-Shield Felt AG Composite is an insulation composite system combining the high temperature use limits of fiber felts with the low thermal conductivity benefits of microporous insulation. The insulation system is comprised of K-Shield Felt AG and a Min-K microporous core. The two materials are quilted together. This composite offers several key advantages over either a traditional microporous material, or a quilted fibrous material, while maintaining the low thermal conductivity (shown below) typically seen in microporous products. The composite insulation system is lighter than comparable Min-K materials. The nominal density of K-Shield Felt AG is 6 pcf, resulting in a final core density of 11 pcf for the 16 pcf Min-K or 7 pcf for the 8 pcf Min-K material, while the thermal conductivity stays virtually constant. Flexible Min- K consists of a microporous core and an outer-textile facing that ypically determines the temperature use limit. High temperature cloths, >1200°F (649°C) are often very costly but by using the K-Shield Felt AG on the hot face, the additional cost of cloth may be eliminated. Due to the fibrous nature of ½ the thickness of these composites, costly edge binding may be eliminated in some instances. By employing the K-Shield Felt AG on the Hot Face, the composite can be used at temperatures greater than the standard maximum temperature use limit of the microporous core. The acoustic properties of Min-K and the K-Shield Felt AG are complementary as each material offers good sound absorption characteristics at different frequencies.

Applications:

  • Glass feeder bowl backup insulation
  • Aluminum transfer troughs
  • Hot metal slag runner systems
  • High-temperature caulking

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors:
Available Properties
  • Density, nominal
  • Thermal Conductivity, ASTM C 201, at 8 pcf
  • Thermal Conductivity, ASTM C 201, at 11 pcf
  • Thermal Conductivity, ASTM C 201, at 11 pcf
  • Thermal Conductivity, ASTM C 201, at 8 pcf
  • Thermal Conductivity, ASTM C 201, at 11 pcf
  • Thermal Conductivity, ASTM C 201, at 11 pcf
  • Thermal Conductivity, ASTM C 201, at 8 pcf
  • Thermal Conductivity, ASTM C 201, at 8 pcf
  • Melting Point
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.