MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
SunChemical Gwent C2100419D1 Copper Paste
Categories: Fluid; Metal; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: This product has been designed as a copper ink for use in termination and circuit printing on ceramic substrates. This product contains a glass frit so may not be suitable for internal electrodes. This product is in a ready to use form at a viscosity suitable for automatic or semi-automatic screen printing.
Economical, lead-free formulation for ceramic applications
Screen Printing Equipment: semi-automatic, manual
Screen Types: stainless steel, polyester, mesh 200-230 tpi
Substrate: Ceramic, Barium Titanate, alumina

Information provided by Gwent Electronic Materials Ltd.

Vendors:
Available Properties
  • Solids Content, in N2
  • Viscosity, Haake VT 550 PK1.1°
  • Storage Temperature, sealed container
  • Surface Resistivity per Square, printed through 230 ss mesh with 13 µm emulsion
  • Sintering Temperature, non-oxygen and reducing atmosphere
  • Cure Time
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Gwent Electronic Materials Ltd.

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.