MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Eastman XIR 7247 Low Iron 6mm
Categories: Polymer; Film

Material Notes: Clear, neutral XIR72-47 laminated film protects interior environments from intense solar energy without the need for darkly tinted or reflective glass. This high performance solar control glass may look like clear glass, but it provides superior protection, energy savings, and comfort. XIR 74-47 performance is created by a thin spectrally selective coating which is applied onto optically clear polyester to make XIR solar control film. XIR’s solar performance and appearance can be adjusted to meet specific design requirements by using tinted glass as the inner lite of the laminated structure, as shown in the table on the reverse page. Because XIR 72-47 can be produced quickly, shipped easily, and inventoried by local laminators it can be readily available for those fast-track projects. With maximum daylighting and minimal solar heat gain, XIR 74-47 laminated film boasts proven sustainability and has been incorporated into some of the most sophisticated projects in the world. The possibilities are now limited only by your imagination.

Benefits:

  • Daylighting-72% light transmittance enable daylighting strategies
  • Energy Savings – SHGC as low as 0.32. SHGC 0.50 with clear glass
  • Transparent Appearance – 8% visible reflectance
  • Reduce Fading – Blocks more than 99% of harmful UV radiation
  • Uniform Appearance – Similar appearance on flat and curved glass – unlike coated glass
  • Reduce Noise Pollution – Superior laminated glass acoustic performance
Applications:
  • All facades
  • Fixed point glazing
  • Storefronts
  • Atriums
  • Skylights
  • Panoramic views
  • Control towers
  • Sports complexes
  • Bent glass

Information provided by Eastman

Vendors:
Available Properties
  • Transmission, Visible, Solar Total
  • Transmission, Visible, Daylight Total
  • Reflection Coefficient, Visible (0-1), Daylight Reflectance, Ext
  • Reflection Coefficient, Visible (0-1), Daylight Reflectance, Int
  • Reflection Coefficient, Visible (0-1), Solar Reflectance, Ext
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.