MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Wacker Elastosil® LR 3015/50 FR A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: ELASTOSIL® LR 3015/50 A/B liquid silicone rubber is a paste like, readily pigmentable two-component compound with extremely short curing time. Its vulcanizates are noted for their high oil resistance. They are colored off white and have moderate mechanical properties. Thanks to the excellent compression set, there is no need to post-cure technical parts.

Application: ELASTOSIL® LR 3015/50 A/B is particularly suitable for the economical production of large series of injection molded articles. Parts made from ELASTOSIL® LR 3015/50 A/B can generally be used for technical applications without post-curing, but do not comply with regulations concerning use in the pharmaceutical and food industry. Due to their high oil resistance, ELASTOSIL® LR 3015/50 A/B is mainly used to produce gaskets for automotive and other mechanical engineering applications.

Information provided by Wacker Chemie AG.

Vendors:
Available Properties
  • Density, DIN EN ISO 1183-1 A
  • Viscosity, DIN 53019
  • Hardness, Shore A, DIN 53505, Oil immersion (70h/150°C), IRM 903
  • Hardness, Shore A, DIN 53505, Oil immersion (70h/150°C),Lubrizol OS 206 304
  • Hardness, Shore A, DIN 53505, Oil immersion (70h/150°C), IRM 901
  • Hardness, Shore A, DIN 53505
  • Tensile Strength at Break, DIN 53504 S 1, Oil immersion (70h/150°C), IRM 903
  • Tensile Strength at Break, DIN 53504 S 1, Oil immersion (70h/150°C),Lubrizol OS 206 304
  • Tensile Strength at Break, DIN 53504 S 1, Oil immersion (70h/150°C), IRM 901
  • Tensile Strength at Break, DIN 53504 S 1
  • Elongation at Break, DIN 53504 S 1, Oil immersion (70h/150°C),Lubrizol OS 206 304
  • Elongation at Break, DIN 53504 S 1, Oil immersion (70h/150°C), IRM 903
  • Elongation at Break, DIN 53504 S 1, Oil immersion (70h/150°C), IRM 901
  • Elongation at Break, DIN 53504 S 1
  • Tear Strength, ASTM 624 B
  • Compression Set, DIN ISO 815-B
  • Maximum Service Temperature, Air, with heat stabilizer
  • Minimum Service Temperature, Air
  • Cure Time, in press
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.