MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Cabot ENDURE™ E37 Carbon Black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: General Description: Many industrial rubber product applications operate under severe conditions that lead to significant wear and tear. Improved durability of the rubber components may provide a distinct total cost advantage. As part of Cabot’s ongoing commitment to deliver solutions that meet our customers’ needs, we have developed the ENDURE™ family of carbon blacks engineered for durability. Improving wear, chunking and tear resistance or reducing heat buildup can result in longer part life, reducing costly equipment downtime, increasing throughput and enhancing end user profitability. Cabot products can enhance rubber part life and durability by optimizing the balance between heat buildup and reinforcement and are identified by the letter “D” in the ENDURE nomenclature system. In certain applications such as conveyor belts, reduced hysteresis in the rubber compound may also be of interest as it can result in decreased power consumption, representing a significant energy and operating cost saving. In other applications such as rubber tracks and certain mill liners, a decrease in hysteresis can help with extending part life. Cabot products can help reduce energy costs and extend part life by optimizing the balance between hysteresis and reinforcement and are identified by the letter “E” in the ENDURE nomenclature system.

Performance Features: ENDURE™ E37 carbon black provides low hysteresis and is relatively easy to disperse with fast incorporation and good dispersion. ENDURE™ E37 carbon black offers reinforcement similar to compounds made with ASTM N300 series carbon blacks but with a considerable reduction in hysteresis and significantly greater durability than ASTM N500 series carbon blacks.

Typical Applications:

  • Bottom cover of low rolling resistant conveyor belts
  • Base of rubber tracks
  • Tread of rubber tracks

Information provided by Cabot Corporation

Vendors:
Available Properties
  • Hardness, Shore A
  • Tensile Strength at Break
  • Elongation at Break
  • 100% Modulus
  • 300% Modulus
  • Rebound
  • Tear Strength
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.