MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
SEKISUI SPI KYDEX® 152WG Wood-capped Thermoplastic
Categories: Polymer; Thermoplastic

Material Notes: Capped wood grain sheet for flat and membrane pressed applications

Super tough, durable KYDEX® 152WG sheet brings new dimensions to membrane pressers in: extensibility, rigidity, abrasion resistance and fire retardancy

This high performance thermoplastic sheet is available in several aesthetically pleasing woodgrain patterns; each substrate color is custom matched to compliment the woodgrain cap. It rates Class I/A when tested according to the ASTM E-84, the Steiner Tunnel Test, and V-0 when independently tested to Underwriters Laboratories, Inc® Std 94 testing.

Suggested Applications:

  • Exhibits & Displays
  • Kiosk Housings
  • Miscellaneous Applications
  • Store Fixture Components
  • Contract Furniture Components

Features:

  • More rigid than most thermoplastics so parts will deform less when loaded
  • Outstanding resistance to breakage
  • Superior scratch and abrasion resistance as evidenced by Hoffman Scratch and Taber Abrasion tests
  • Substrate of complimentary color camouflages gouges
  • Rated class I/A according to ASTM E-84 Tunnel Test in independent laboratory testing (thicknesses less than 1.00 mm (0.040 in))
  • Rated V-0 in all thicknesses and colors when independently tested to Underwriter's Laboratories, Inc® Standard 94
  • Available in 13 popular wood grain patters

Values based upon 3.18 mm (0.125 in) sheet unless otherwise specified.

Information provided by Sekisui Polymer Innovations

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Tensile Strength, ASTM D638
  • Modulus of Elasticity, ASTM D790
  • Flexural Strength, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Abrasion, Hoffman Scratch Test, g
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Annealed
  • Flammability, UL94, UL Standard 94, Independent Laboratory Testing
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.