MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Syensqo (Solvay Specialty Polymers) Hyflon® MFA 1041 Perfluoroalkoxy (PFA)
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA); Polyperfluoroalkoxyethylene, Molded/Extruded

Material Notes: Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent fire characteristics, physical properties, and processing. The unique chemical structure of MFA provides the superior properties necessary for the increasingly demanding telecommunications industry.

Cables manufactured with MFA 1041 have met the Telecommunications Industry Association (TIA) Category 6 standard. The extremely low attenuation of MFA 1041 makes it a logical choice for the developing Augmented Category 6 standard. Cables made from MFA 1041 have met the fire performance requirements called out in NFPA 90a ("Standard for Air- Conditioning and Ventilating Systems").

Hyflon® MFA 1041 is not recommended for heavy wall applications where significant thermal stress crack resistance is required.

Applications: Telecommunications; Tubing; Wire & Cable Applications

Features: Flame Retardant; Good Electrical PropertiesSolvay recommends that only Color Master Batches based in MFA 1041 be used. Master Batches based on other fluoropolymers can negatively influence the superior processing and electrical performance of MFA 1041. A list of suppliers can be obtained from your Solvay sales representative.

HEALTH SAFETY AND ENVIRONMENT
- Hyflon MFA 1041 is a very inert polymer and it is not harmful if used and handled according to standard processing procedures. If handled inappropriately, it may release harmful toxic chemicals. MFA also complies with Directive 2002/95/EC ("Restrictions of hazardous substances in waste from electrical and electronic equipment" - RoHS), Directive 2000/53/EC ("End of life of vehicles" - ELV) and Directive 76/769/EEC ("Restrictions on the marketing and use of certain dangerous substances and preparations"), as subsequently amended.

PACKAGING AND STORAGE
- Hyflon MFA 1041 resin is available in 25 kg (55 lbs.) and 500 kg (1102 lbs.) packaging. Though it has an indefinite shelf life, it is recommended to store it in a clean area, protected by direct sun light and possible contamination.

Extrusion notes: WIRE AND CABLE PROCESSING GUIDELINES
- As with other fluoropolymers, Hyflon MFA is corrosive in the melt. Therefore all parts coming into prolonged contact with the melt should be made with corrosion resistant materials such as Hastelloy®, Inconel®, Monel® or Xaloy®. Chrome or nickel plating is not recommended since they are typically only sufficient for brief processing tests.
- MFA 1041 is applied onto wire using tubing extrusion techniques similar to other thermoplastic materials. An overview of the temperature, tooling and equipment requirements are in the following tables.
- MFA can be processed with many different screw designs. Single-flight screws are recommended while barrierflights should be avoided. A typical screw design consist of a long feed section, followed by a 2 to 6 flight transition and a 5 to 7 flight metering section. The addition of a Saxton mixing or other block mixing sections can improve the processing performance.
EQUIPMENT/TOOLING REQUIREMENTS
- Line Speed: 1,500-2,500 ft/min (450-750 m/min)
- Draw Down Ratio: 80-120
- Draw balance: 0.98-1.05
- Extruder: L/D 24/1-30/1
- Screen pack: Breaker plate only is required

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow, ASTM D1238
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638, 1.0 mm/min
  • Izod Impact, Notched, ASTM D256
  • Volume Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • Heat of Fusion, DSC
  • CTE, linear, Parallel to Flow, ASTM D696
  • Specific Heat Capacity, ASTM C351
  • Thermal Conductivity, ASTM C177
  • Melting Point
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  • Zone 1, Extrusion
  • Zone 2, Extrusion
  • Zone 3, Extrusion
  • Zone 4, Extrusion
  • Zone 5, Extrusion
  • Adapter Temperature, Extrusion
  • Die Temperature, Extrusion
  • Melt Temperature, Extrusion
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

http://www.madehow.com/Volume-1/Tire.html
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.