MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
Clariant Natural Color Polyethylene Terephthalate Glycol 3D Printer Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Material Notes: Glycol modified polyethylene terephthalate (PET-G) is a polyester with good toughness and chemical resistance. 3D printed PET-G exhibits good layer adhesion and can be used to produce all kinds of products which include end use parts, prototypes, jigs, and fixtures. Clariant improves the heat stability and resistance to thermal processes using appropriately selected additives such as Hostanox® P-EPQ® and Hostavin® ARO 8.

General properties:

  • Strong and tough engineering thermoplastic
  • Transparent
  • Good impact strength
  • Good chemical resistance
Optimized benefits:
  • Reduced thermo-oxidative degradation
  • Minimized undesired yellowing due to ultraviolet light
Applications:
  • Prototypes
  • Tools, jigs, fixtures
  • Containers / packaging
  • Mechanical and technical application parts

Information provided by Clariant.

Vendors:
Available Properties
  • Density, ISO 1183
  • Melt Flow, ISO 1133
  • Tensile Strength at Break, ISO 527, Injection molded, 50 mm/min
  • Tensile Strength, Yield, ISO 527, Injection molded, 50 mm/min
  • Elongation at Break, ISO 527, Injection molded, 50 mm/min
  • Flexural Modulus, ISO 178, Injection molded
  • Izod Impact, Notched (ISO), ISO 180, Injection molded
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75, Injection molded
  • Glass Transition Temp, Tg, ISO 11357, DSC
  • Transmission, Visible, Transparent but manufacturer does not quantify
  • Processing Temperature, Print Temperature
  • Moisture Content, ISO 15512, after drying at 120°C for 2 hours
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.