MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Epoxy Technology EPO-TEK® E4110-PFC Electrically Conductive Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: Product Description: EPO-TEK®E4110-PFC is a two-component, silver filled, electrically conductive adhesive designed for semiconductor IC packaging and general electronic assembly. It is a thixotropic version of EPO-TEK®E4110, suggested for applications requiring a screen printing process as well as jetting.

Advantages & Application Notes:

  • A thixotropic paste which enables ultra-fine pitch applications at the wafer or PCB/substrate packaging level. It may be dispensed, printed or jetted.
  • Semiconductor Flip Chip Suggested Applications:
    • Flip Chip attaching of IC’s direct to substrate or in semiconductor advanced plastic packages.
    • “Dots” of E4110-PFC may be realized at 75µm diameter and 125µm pitch.
    • Compatible with screen printing processes, whether mesh or stencil foils. The former requires > 200 mesh wires while the latter should be laser etched SST foil.
    • Capable of curing at temperatures as low as 45°C for solder replacement.
  • Medical Suggested Applications:
    • Electrically conductive bridge when bonding Au-plated piezo-ceramic arrays to PCBs, used in ultrasonic devices.
    • Flip chip attachment of photo-detector arrays found in X-ray and CT detectors
  • Opto-electronics Suggested Applications
  • Electrically conductive adhesive found in sensor and fiber optic devices
  • Electrical bridge of ITO contact pads to PCBs found in LCD/Displays and OLED’s
  • Flex Circuits suggested Applciations.
    • Solar / Photo-voltaic. Adhesive for electrically back-contacting, thin film, organic and dye sensitized solar cells.
    • Flip Chip adhesive dots bridging RFID chips to antennae, or smart card IC packaging.
    • Electrical bridge of Au/PZT arrays to Au/Kapton found on ink-jetting circuits

    Information Provided by Epoxy Technology

  • Vendors:
    Available Properties
    • Specific Gravity, Part B
    • Specific Gravity, Part A
    • Particle Size
    • Viscosity, 5 rpm
    • Ionic Impurities - Na (Sodium)
    • Ionic Impurities - K (Potassium)
    • Ionic Impurities - Cl (Chloride)
    • Hardness, Shore D
    • Tensile Modulus, Storage
    • Shear Strength, Lap
    • Shear Strength, Die
    • Volume Resistivity
    • CTE, linear, Below Tg
    • CTE, linear, Above Tg
    • Thermal Conductivity
    • Maximum Service Temperature, Air, Continuous
    • Maximum Service Temperature, Air, Intermittent
    • Minimum Service Temperature, Air, Continuous
    • Minimum Service Temperature, Air, Intermittent
    • Glass Transition Temp, Tg, Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
    • Decomposition Temperature, TGA, Degradation Temperature
    • Cure Time, Minimum Bond Line
    • Cure Time, Minimum Bond Line
    • Cure Time, Minimum Bond Line
    • Pot Life
    • Shelf Life
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    Plastic

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Chemically Resistant adhesives
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.