For all products containing Flame additives Rhodia recomends the use of high Chromium, low Carbon coating for the steels (example CR19% C1.9%). The use of this steel can help to prevent corrosion, extend the equipment lifetime and allow greater parameter flexibility.
Information provided by Rhodia; Rhodia has been acquired by Solvay.
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticPA, Polyamide