MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Eastman EASTALLOY Polymer DA105, Natural Alloy  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: General: All ISO tests are run @ 4-mm thickness with the exception of Impact Resistance, which is run @ 2-mm thickness.

Comments: Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform to the values give

Information provided by Eastman Chemical.

Vendors:
Available Properties
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength, Ultimate, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Flexural Yield Strength, ISO 178
  • Flexural Yield Strength, ASTM D790
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • Electrical Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • Dielectric Constant, ASTM D 150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, Short Time, 500 V/sec rate-of-rise; ASTM D 149
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • Arc Resistance, ASTM D495
  • Comparative Tracking Index, ASTM D3638
  • High Voltage Arc-Tracking Rate, HVTR, UL 746A
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648 and ISO 75
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648 and ISO 75
  • Vicat Softening Point, 5 kg load; ISO 306
  • Vicat Softening Point, 1 kg load; ISO 306
  • Flammability, UL94
  • Flammability, UL94
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.