MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
DuPont Teijin Films Mylar® OL22 Polyester Film, 100 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Product Description: Mylar® OL22 is a one side heat sealable, polyester film. It can be heat sealed to itself and heat seals well to thermoformed APET/CPET trays and APET coated board. It also heat seals to various other substrates including PVdC, PVC, paper and aluminum foil, but will not seal to polyolefins. The plain or non-heat seal surface of Mylar® OL22 exhibits the properties of standard polyester film.

General Product Info: Mylar® OL22 has an exceptionally wide heat seal range, from 220°F to 400°F, with outstanding hot tack properties. The plain surface of Mylar® OL22 can be printed or metallized in the same way as plain polyester film, although the sealable surface makes handling of the film during conversion more critical. The heat seal surface of the film is normally wound on the inside of the roll.

Typical Applications: Mylar® OL22 is an excellent film for applications where chemical resistance of the sealant surface is required. It offers excellent thermal properties in freezer to oven applications for lidding applications.

Approvals: FDA Food Contact Status - All gauges of Mylar® OL22 comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers. This regulation describes films which may be safely used in contact with all types of food excluding alcoholic beverages. Mylar® OL22 can be used to contain foods during oven cooking or oven baking at temperatures above 250 °F.

Information provided by DuPont.

Vendors:
Available Properties
  • Density, ASTM D1505, Typical Mylar®
  • Water Vapor Transmission, ASTM F1249, 90% RH
  • Thickness
  • Film Elongation at Break, MD, ASTM D882A
  • Film Elongation at Break, TD, ASTM D882A
  • Coefficient of Friction, Dynamic, ASTM D1894
  • Film Tensile Strength at Break, MD, ASTM D882A
  • Film Tensile Strength at Break, TD, ASTM D882A
  • Heat Seal Strength, 285°C (HS/HS)
  • Specific Heat Capacity, Typical Mylar®
  • Melting Point, Typical Mylar® via DSC
  • Shrinkage, MD, Unrestrained
  • Shrinkage, TD, Unrestrained
  • Refractive Index, typical of Mylar®
  • Haze, ASTM D1003
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
DuPont Teijin Films

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.