MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chesterton Opticoolâ„¢ 372 Metalworking Fluid
Categories: Fluid; Lubricant

Material Notes: Description: OPTICOOL 372 is a proven, universal, water miscible metal working fluid. It is ideal where lubricity is important and operations severe. The 372 is suitable for a broad range of metal cutting operations. When mixed with water, 372 forms a stable, emulsion providing for effective machining operations. OPTICOOL 372 improves productivity by reducing the time to process metals, increasing the quality of the workmanship and increasing tool life. 372 offers cost effective dilution rates, corrosion inhibiting properties, extreme pressure additive package and hard water stability.

Properties:

  • Stable emulsion for long lasting use
  • Unique base oil technology
  • Extreme pressure capability
  • Minimizes rancidity and odors
  • Lowers disposal and downtime costs
  • Corrosion protection
  • Virtually eliminates adverse skin effects

Suggested Uses:

  • Braoching
  • Deep Drilling
  • Reaming
  • Sawing
  • Tapping
  • Fine Threading
  • Milling
  • Turning
  • Grinding
  • Stamping
  • Drawing

    Information provided by Chesterton

Vendors:
Available Properties
  • Specific Gravity
  • pH, 10% Concentration
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.