Initiator (75% water in powder) for the production of PVC, PVA, PVOH and acrylics. CAS number: 15520-11-3 EINECS/ELINCS No.: 239-557-1 Applications: Polymerization of vinyl chloridePerkadox 16-W75 is applied as an initiator for the suspension and mass polymerization of vinyl chloride in the temperature range between 40°C and 65°C. Perkadox 16-W75 can be used alone or in combination with other peroxides, such as 1,1,3,3-Tetramethylbutyl peroxyneodecanoate (Trigonox 423), Cumyl peroxyneodecanoate (Trigonox 99) or Dilauroyl peroxide (Laurox), to increase reactor efficiency. Information provided by Nouryon |