MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Hybrid Plastics MS0825 Nanoreinforced® POSS® Polyamide 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Nanoreinforced® polyamide 6 (PA6) utilizes POSS® technology to achieve increased hydrophobicity, increased oil resistance, improved toughness and easier processability through structural control at the nanometer level. POSS’s nanoscopic size, dispersion, and chemical structure lead to these enhancements which can be realized in any grade of polyamide.

Mechanism of Modification: The hydrophobic properties of POSS® synergistically combines with polyamide morphology to create a nano-rough surface that is both hydrophobic and low friction. The technique is ideally suited to masterbatching.

Enhanced hydrophobicity is observed by water contact angle differences for PA6 and Nanoreinforced® PA6. Water contact angle increases with POSS® content, and follows standard rules of mixing when let down from a masterbatch.

Lower water uptake results from the enchanced hydrophobicity and durability increases by reducing hydrolytic degradation. Faster processing results from a lubricity effect that is imparted by the POSS and increases melt flow and decreases the screw torque required during compounding and during masterbatch let down.

Increased toughness is observed at low loadings of POSS®. Other mechanical characteristics are maintained or improved compared to that of the base polyamide resin grade. Suggested Applications textiles, packaging, film and fiber applications

Vendors:
Available Properties
  • Water Absorption at Saturation, 15% POSS® loading (vs. 8% water absorption for neat nylon 6)
  • Water Absorption at Saturation, 3% POSS® loading (vs. 8% water absorption for neat nylon 6)
  • Tensile Strength at Break, 3% MS0825 addition (vs. 30 MPa for neat Nylon 6)
  • Tensile Strength at Break, 5% MS0825 addition (vs. 30 MPa for neat Nylon 6)
  • Tensile Strength at Break, 10% MS0825 addition (vs. 30 MPa for neat Nylon 6)
  • Elongation at Break, 3% MS0825 addition (vs. 80% for neat Nylon 6)
  • Elongation at Break, 5% MS0825 addition (vs. 80% for neat Nylon 6)
  • Elongation at Break, 10% MS0825 addition (vs. 80% for neat Nylon 6)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.