Norylux™ PPO modified Poly Phenylene Oxide is a high-strength, amorphous, engineering plastic with outstanding mechanical, thermal, and electrical properties. Low moisture absorption and low coefficient of thermal expansion make Norylux™ PPO one of the most dimensionally stable thermoplastics available. Norylux™ PPO is widely used for electrical housings and structural components since it has excellent insulating properties, flame resistance, strength and stiffness, and dimensional stability over a wide range of service temperatures. Norylux™ PPO is often selected for fluid handling applications since it has low moisture absorption and hydrolytic stability. Norylux™ PPO machines easily and may be fabricated into complex shapes with close tolerances. Norylux™ PPO is also easy to weld and glue, and it provides good adhesion to paints, inks, and other decorative coatings. Westlake Plastics extrudes and compression molds unfilled and flame-retardant products and compression molds glass reinforced and glass/mineral filled products. Colors Available: Black Attributes: Dimensional Stability; Good Contact; Impact Resistance; Dielectric Properties Shapes: Compression Sheet; Extruded Sheet; Extruded Film; Extruded Rod. Available rod diamters are 0.5", 0.625", 0.75", 0.875", 1", 1.25", 1.375", 1.5" , 1.625", 1.75", 1.875", 2", 2.25", 2.5", 2.75", 3", 3.25", 3.5", 3.75", 4", 4.25", 4.5", 4.75", 5" Information provided by Westlake Plastics Co. |