MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Wacker Wacker® E60 1000 Silicone Emulsion
Categories: Polymer; Thermoset; Silicone

Material Notes: Product description: E60 1000 is a 60% silicone emulsion using a nonionic surfactant system.

Special features:

  • Long term dilution stability
  • Ease and versatility of application
  • Relatively non-reactive
  • Absence of fire hazard
  • Ease of application and rub out
  • Excellent shear and lubricating
  • Lower inventory costs; requires less handling, storage and shipping
  • Less material required to achieve the intended effect
  • Lower costs on silicone solids
Application: E60 1000 has been designed to be used in many applications, such as mold release, textile lubricants and softeners, automotive care, and other specialty product applications. It is an excellent product for a formulator who can easily repackage and sell at lower concentrations. It can be used in either the concentrated or diluted form and can be combined with many organic thread lubricants and softeners. In mold release applications, E60 1000 is very effective at low dilution levels (0.5 - 2.0% silicone). It gives a very quick and easy release of rubber and plastic parts.

Information provided by Wacker Chemie AG.

Vendors:
Available Properties
  • Density
  • Viscosity
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.