MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Gouda Refractories Pinnacle PP 1635AF PP Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Product Description: 35 melt flow homopolymer. Pinnacle Polymers Polypropylene 1635AF is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties and lot-to-lot consistency. This product is intended for injection molding; the flow properties should be of particular benefit in the production of thin-walled articles. It contains no nucleators, antistats or animal derivatives. Potential applications include: healthcare/medial packaging, labware, containers and thin-wall articles in general.
Features: Heat Sterilizable (autoclavable); Contains no animal derivatives; Excellent color and processing stability; Low Extractables
Pinnacle’s 1635AF polypropylene as marketed by Pinnacle Polymers Company, in natural, uncolored pellet form complies with appropriate requirements of CFR Title 21, Part 177, Subpart B, Section 177.1520 © 1.1a entitled “Olefin Polymers” of the Food Additives Amendment of 1958 to the United States Food, Drug and Cosmetic Act of 1938.

Availability: Europe; North America

Features: Autoclavable; Food Contact Acceptable; Good Color Stability; Good Process Stability; Heat Sterilizable; Homopolymer; Low Extractables; No Animal Derived Components

Uses: Containers; Labware; Medical Packaging; Thin-walled Parts

Agency Ratings: FDA 21 CFR 177.1520 © 1.1a

Appearance: Natural Color

Form: Pellets

Processing Method: Injection Molding

Information provided by Pinnacle Polymers

Vendors:
Available Properties
  • Density, ASTM D1505
  • Melt Flow, ASTM D1238
  • Tensile Strength, Yield, ASTM D638, Injection Molded, Type I, 2.0 in/min
  • Elongation at Break, ASTM D638, Injection Molded, Type I, 2.0 in/min
  • Flexural Modulus, ASTM D790A, 1% Secant, Injection Molded, Type I, 0.05 in/min
  • Izod Impact, Notched, ASTM D256, Injection Molded, Type I
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Gouda Vuurvast

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.