MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Zell-Metall Engineering Plastics Zellamid 250 (PA6.6)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Zellamid® 250 is noted for its high temperature resistance and high tensile strength. It is the hardest and most rigid type of extruded Nylon. Main characteristics are high resistance to fuels, oils, greases, most organic solvents and alkalis. Moisture absorption is lower than for Nylon 6.

Typical applications are friction bearings, gears, cams and cam followers, guides, sleeves, valve seats and articles subjected to high loads and/or for high temperature.

Vendors:
Available Properties
  • Density
  • Moisture Absorption at Equilibrium, ISO 1110; DIN 53714, 50% RH
  • Water Absorption at Saturation, ISO 62; DIN 53495, 23°C
  • Ball Indentation Hardness, ISO 2039; DIN 53456, H 358/30
  • Tensile Strength at Break, ISO 527; DIN 53455
  • Elongation at Break, ISO 527; DIN 53455
  • Tensile Modulus, ISO 527; DIN 53452
  • Izod Impact, Notched, ISO 180 Method A
  • Charpy Impact Unnotched, ISO 179; DIN 53453
  • Charpy Impact Unnotched, ISO 179; DIN 53453
  • Charpy Impact, Notched, DIN 53753, double V-notch, rk=1.5 mm
  • Dart Drop, Total Energy, DIN 53443
  • Dart Drop, Total Energy, DIN 53443
  • Volume Resistivity, IEC 167; DIN 53482
  • Surface Resistance, IEC 167; DIN 53482
  • Dielectric Constant, IEC 250; DIN 53483
  • Dielectric Strength, IEC 243; DIN 53481
  • Dissipation Factor, IEC 250; DIN 53483
  • Comparative Tracking Index, IEC 112; DIN 53480, KB Method
  • Comparative Tracking Index, IEC 112; VDE 0303T1, KC Method
  • CTE, linear, DIN 53752
  • Specific Heat Capacity, DIN 52612
  • Thermal Conductivity, DIN 53612 Method A
  • Melting Point, ISO 1218 Method A; DIN 53736
  • Maximum Service Temperature, Air, IEC 216; DIN 53446, 20,000 hours; 50% Tensile Strength
  • Maximum Service Temperature, Air, IEC 216; DIN 53446, 5000 hours; 50% Tensile Strength
  • Maximum Service Temperature, Air, a few hours operation
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75; DIN 53461
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75; DIN 53461
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.