MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
CHT Group QM 140T 40 Shore A, Translucent, Condensation Cure Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QM 140T is a two-component, translucent, room temperature, condensation cure, silicone material. This material was specifically designed for vacuum bagging applications. When catalyzed with QM Cat Clear Thixo 2 the resulting material is extremely thixotropic. QM 140T is also available for non-thixotropic, flowable, applications when catalyzed with QM Cat Clear. The cured rubber has excellent properties and good shelf life stability.

Key Features:

  • High tear strength
  • High thixotropy (if desired)
  • Fast demold time
  • Excellent dimensional stability
Main Applications:
  • Molds for polyester, polyurethane and epoxy resin castings
  • Designed specifically for vacuum bag applications

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors:
Available Properties
  • Specific Gravity, Uncatalyzed Cat Clear
  • Specific Gravity, Uncatalyzed Clear Thixo 2
  • Specific Gravity, Catalyzed Cat Clear
  • Specific Gravity, Catalyzed Clear Thixo 2
  • Specific Gravity, Uncatalyzed QM 130T
  • Viscosity, Uncatalyzed Cat Clear
  • Viscosity, Uncatalyzed Clear Thixo 2
  • Viscosity, Uncatalyzed QM 130T
  • Linear Mold Shrinkage, Cured 3 days RT, Cat Clear
  • Linear Mold Shrinkage, Cured 3 days RT, Catalyzed Clear Thixo 2
  • Hardness, Shore A, Cured 3 days RT, Cat Clear
  • Hardness, Shore A, Cured 3 days RT, Catalyzed Clear Thixo 2
  • Tensile Strength, Cured 3 days RT, Catalyzed Clear Thixo 2
  • Tensile Strength, Cured 3 days RT, Cat Clear
  • Elongation at Break, Cured 3 days RT, Catalyzed Clear Thixo 2
  • Elongation at Break, Cured 3 days RT, Cat Clear
  • Tear Strength, Cured 3 days RT, Catalyzed Clear Thixo 2
  • Tear Strength, Cured 3 days RT, Cat Clear
  • Maximum Service Temperature, Air, Cured 3 days RT, Cat Clear
  • Maximum Service Temperature, Air, Cured 3 days RT, Catalyzed Clear Thixo 2
  • Minimum Service Temperature, Air, Cured 3 days RT, Cat Clear
  • Minimum Service Temperature, Air, Cured 3 days RT, Catalyzed Clear Thixo 2
  • Cure Time, Demold time, Catalyzed Clear Thixo 2
  • Cure Time, Demold time, Catalyzed Cat Clear
  • Cure Time, Cat Clear
  • Cure Time, Catalyzed Clear Thixo 2
  • Tack-Free Time, Catalyzed Clear Thixo 2
  • Tack-Free Time, Catalyzed Cat Clear
  • Pot Life, Catalyzed Cat Clear
  • Pot Life, Catalyzed Clear Thixo 2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.