Key features of this grade: Thixotropic, high flash point, low emissions, excellent tank stability. VOC-free. Vacuum pressure impregnation (VPI) is mainly used when the penetration and filling factor of the resin need to be improved versus other processing options. Information provided by Von Roll. |