MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); 80% Cold Work
Categories: Metal; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Material Notes: Mechanical property data for cold rolled bar aged 900°F (482°C) for 20 hours.

High-Strength, Oxidation Resistant Strip Alloy

Features: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aerospace applications include engine exhaust plug and nozzle assemblies. The alloy's resistance to aircraft hydraulic fluids, such as Skydrol, is excellent at all temperatures. It is well suited for metal matrix composites because it can be economically rolled to foil, is compatible with most fibers, and is sufficiently stable up to 816°C.

Typical heat treatment for this alloy: Solution treatment: 816-843°C (1500° - 1550°F) for 3-30 min, air cool. Age treatment: 510-679°C (950° - 1275°F) for 8-16 hrs.

Data provided by TIMET.

Key Words: Beta 21S; UNS R58210
Vendors:
Available Properties
  • Density, Typical
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity, Aged 1000°F (538C) for 8 hours
  • Electrical Resistivity, Aged 1000°F (538°C)
  • Electrical Resistivity, Aged 1000°F (538°C)
  • Electrical Resistivity, Aged 1000°F (538°C)
  • Electrical Resistivity, Aged 1000°F (538°C)
  • CTE, linear, Aged 1000°F (538°C)
  • CTE, linear, Aged 1000°F (538°C)
  • CTE, linear, Aged 1000°F (538°C)
  • CTE, linear, Aged 1000°F (538°C)
  • CTE, linear, Aged 1000°F (538°C)
  • CTE, linear, Aged 1000°F (538°C)
  • CTE, linear, Aged 1000°F (538°C)
  • Specific Heat Capacity, Aged 1000°F (538°C)
  • Specific Heat Capacity, Aged 1000°F (538°C)
  • Specific Heat Capacity, Aged 1000°F (538°C)
  • Specific Heat Capacity, Aged 1000°F (538°C)
  • Thermal Conductivity, Aged 1000°F (538°C)
  • Thermal Conductivity, Aged 1000°F (538°C)
  • Thermal Conductivity, Aged 1000°F (538°C)
  • Thermal Conductivity, Aged 1000°F (538°C)
  • Maximum Service Temperature, Air, Structural Applications
  • Beta Transus
  • Aluminum, Al
  • Carbon, C
  • Hydrogen, H
  • Iron, Fe
  • Molybdenum, Mo
  • Niobium, Nb (Columbium, Cb)
  • Nitrogen, N
  • Other, each
  • Other, total
  • Oxygen, O
  • Silicon, Si
  • Titanium, Ti, Calculated as remainder
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.