LNP THERMOCOMP RX10405H compound is based on Nylon 6/6 resin containing 40% carbon fiber. Added features of this grade include: Electrically Conductive, Healthcare. Features: Healthcare,High Stiffness,Light-weight Structural,Super Strong (Carbon Fiber Filled),Electrically Conductive,Structural Information provided by SABIC |