MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Polimersan Plastics POLITEF® (PTFE)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of its strong connection between the carbon and fluor atoms and its molecular structure made of a long and linear carbon chain, which is full with fluor atoms.

It has the widest working heat interval among all the industrial plastics (-260°C and +260°C) , complete unlimited resistance against humidity, against environment conditions and against all the chemical materials used in industry. It has the lowest static and dynamic friction coefficient among all the known solids, superior electrical isolation, non-adhesiveness, non inflammability and other properties like these. In addition to these, it has sufficient mechanical properties and full resistance against all chemical materials. All these provide POLITEF to be preferred more than the other materials at many usage areas. Moreover many times only POLITEF is being used.

POLITEF, is a material which can be used at many fields because of its above mentioned properties. Medicine, air and space technologies, cable and cable structure groups at computer sector, filter products, systems for determining leakage, valve spare parts, mechanical spare parts, electrical industry, food industry and textile industry are only small examples of POLITEF`s usage areas.

Information provided by Polimersan Polimer Kimya San.Tic.Ltd.Sti.

Vendors:
Available Properties
  • Specific Gravity, ASTM D1457-18; ISO.1183 DN.53479
  • Deformation, ASTM D621, 230°C, 1 day, 140 kg/cm^2
  • Hardness, Shore D, ASTM D2240; DIN.53505
  • Ball Indentation Hardness, ISO.2039-2
  • Tensile Strength, Yield, ASTM D1708
  • Tensile Strength, Yield, ISO.527 DN.53455
  • Elongation at Break, ASTM D1708
  • Elongation at Yield, ISO.527 DN.53455
  • Izod Impact, Notched, ASTM D256
  • Volume Resistivity, ISO.167 DN.53482
  • Surface Resistance, ISO.167 DN.53482
  • Dielectric Strength, ASTM D149; ISO.243 DN.53481
  • CTE, linear, ASTM E831
  • Thermal Conductivity, ASTM C177
  • Melting Point, ISO.3146
  • Maximum Service Temperature, Air, ISO.75 DN.53461
  • Minimum Service Temperature, Air
  • Brittleness Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.